Void bias in irradiated model metals

Figure 8. Specific bias of (A) voids with different sizes and (B) different sinks in Cu, Ni, and Fe. In (B), the SFT has a size of 2 nm, while both the loop and void have diameters of 10 nm. Dislocation loop types are selected based on experimental observations: 1/3<111> Frank loops observations for fcc Cu[57] and fcc Ni[39], and <100> Frank loops for bcc Fe[37].