fig7

Figure 7. Stress-strain curves of PEDOT:PSS/SWCNT composite films with different SWCNT and IL contents at (A) room temperature, (B) 393 K and (C) 470 K. (D) Comparison of elongation at break of composites with and without IL. PEDOT:PSS/SWCNT: Poly(3,4-ethylenedioxythiophene):poly(styrene sulfonate)/single-walled carbon nanotube; IL: ionic liquid.