Incommensurate modulations and thickness-dependent energy storage density in (PbLaSrBa)(ZrSnTi)O<sub>3</sub> relaxor antiferroelectric thick-film ceramics

Figure 6. (A) P-E loops for PLSBZST2 thick-film ceramics at 940 kV/cm from 30 to 110 °C; (B) Corresponding EAFE-FE, EFE-AFE, ΔE, and Pmax values obtained at various temperatures; (C) Calculated Wtot, Wrec, and η values obtained at various temperatures; (D) P-E loops for the PLSBZST2 thick-film ceramic at 880 kV/cm from 0.2 to 100 Hz; (E) Corresponding EAFE-FE, EFE-AFE, ΔE, and Pmax obtained at various frequencies; (F) Calculated Wtot, Wrec, and η values obtained at various frequencies. P-E: Polarization - electric field; PLSBZST2: (Pb0.86La0.04Sr0.06Ba0.02)(Zr0.64Sn0.35Ti0.01)O3; Pmax: maximum polarization; Wtot: total energy storage density; Wrec: recoverable energy storage density.

Microstructures
ISSN 2770-2995 (Online)

Portico

All published articles are preserved here permanently:

https://www.portico.org/publishers/oae/

Portico

All published articles are preserved here permanently:

https://www.portico.org/publishers/oae/