fig5

Incommensurate modulations and thickness-dependent energy storage density in (PbLaSrBa)(ZrSnTi)O<sub>3</sub> relaxor antiferroelectric thick-film ceramics

Figure 5. (A) P-E and (B) current - electric field (I-E) hysteresis loops obtained at room temperature for PLSBZST thick-film ceramics; (C) EAFE-FE, EFE-AFE, ΔE, and Pmax; (D) Weibull distribution of the four samples, with the inset showing the DBS as a function of x; (E) Wrec and η for four samples; (F) Comparison of the Wrec and η values of PLSBZST2 with those of recently reported AFE ceramics[11,29,30,34,35,50-59]. P-E: Polarization - electric field; PLSBZST: (Pb0.92-xLa0.04SrxBa0.02)(Zr0.64Sn0.35Ti0.01)O3; DBS: dielectric breakdown strength; AFE: antiferroelectric; Pmax: maximum polarization; Wrec: recoverable energy storage density.