fig5
Figure 5. (A) Schematic illustration of the preparation procedure of pCu NS; (B) HRTEM image of pCu NS. (A and B) Reproduced with permission[114]. Licensed under CC BY 4.0; Synthesis scheme for (C) Cu-1H-1,2,3-triazole (Cu-triazole) and (D) defect-Cu-1H-1,2,3-triazole (D-Cu-triazole) with their corresponding crystal structure. (C and D) Reproduced with permission[115]. licensed under CC BY 4.0; (E) Schematic illustration on multi-factor interfacial regulation with 3DOM structure, giving faster mass transport, higher local pH, and stronger electric field at the catalyst-electrolyte interface; (F) SEM, TEM, STEM images, and EDS mapping of dendritic Cu0 in 3DOM-La2CuO4-P. (E and F) Reproduced with permission[116]. Copyright 2026, Wiley-VCH. NS: nanosheet; HRTEM: High-Resolution Transmission Electron Microscopy; SEM: Scanning electron microscopy; TEM: Transmission electron microscopy; STEM: Scanning Transmission Electron Microscope; EDS: Energy-dispersive X-ray spectroscopy.