From: Emerging medium-range order in deformed Zr-based bulk metallic glasses during sub-Tg relaxation
Figure 2. (A) Nanoindentation test results for AC, CR, and HPT BMGs. (B) Hardness and modulus of AC, CR and HPT BMGs from nanoindentation. The error bar indicates the standard deviation through eight tests. (C) The surface morphology of the indentation of AC, CR, and HPT BMGs. The scale bar is 5 μm. (D) The load versus displacement curves of BMG pillars. (E) The morphology of the pillars of AC, CR, and HPT BMGs before and after compression tests. The scale bar is 1 μm.