fig3
Figure 3. (A) True stress-strain curve and its corresponding work hardening rate curve of in situ neutron diffraction tensile test; (B) The intergranular lattice strains of alloy for the composite γ + γ′ overlapping FCC peaks; (C) The deconvoluted intragranular (interphase) lattice strains of individual phase in the {200} and {220} reflections. FCC: Face-centered cubic.