 <i>Pseudoalteromonas spongiae</i>-induced biomineralization on Q235B and 2507 steel for corrosion and biofouling resistance

Figure 9. (A) Nyquist plot and (B) Bode plot after 3-day immersion; (C) Macro images and (D) micro morphology of Q235B and 2507 immersed in ASW after 3 days with product removed. ASW: Artificial seawater.