fig19

Unique grain-boundary mediated plasticity: Deep Potential MD insights in HCP zinc

Figure 19. Atomic structure of columnar grain system of (A and D) Zn, (B and E) Mg and (C and F) Be, respectively, corresponding to the peak (A-C) and stable stress (D and E) stages, where the applied strains of A2, B2 and C2 are 7.0%, 6.0% and 6.5%, and A4, B4 and C4 are 19.0%, 18.1% and 19.0%, respectively, at the strain rate of 1 × 1010 s-1. The red, green, blue and white atoms represent HCP, FCC, BCC and other structures, respectively. HCP: Hexagonal close-packed; FCC: face-centered cubic; BCC: body-centered cubic; TB: twin boundary.