Microstructural evolution and fatigue mechanism of 316LN austenitic stainless steel welded joint at 4.2 K

Figure 2. (A) Phases map, (B) Schmid factor map, (C-C3) inverse pole figures, (C4-C6) grain size statistical diagrams, (D) Kernel average misorientation map, and (D1-D3) GND density statistical diagrams of the as-fatigued welded joint. BM: Base material; HAZ: heat-affected zone; FZ: fusion zone; GND: geometrically-necessary dislocation; FCC: face-centered cubic; BCC: body-centered cubic.