Pitting corrosion growth of an Inconel alloy revealed by three-dimensional reconstruction

Figure 8. Growth process of pits on Inconel 690 alloy in 6% FeCl3 + 0.16% HCl solution at 70 °C (A) 9 h, (B) 12 h, (C) 15 h, and (D) 18 h.