fig6

Pitting corrosion growth of an Inconel alloy revealed by three-dimensional reconstruction

Figure 6. Optical micrographs of pits formed by passive film breakdown at non-inclusion sites: (A) Surface of the uncorroded sample; (B) After 1 h of corrosion at 90 °C; (C) After 2 h of corrosion at 90 °C.

Microstructures