Pitting corrosion growth of an Inconel alloy revealed by three-dimensional reconstruction

Figure 19. Comparison of projected and actual pit parameters at 90 °C: (A) Comparison of maximum width after 7 h, (B) Comparison of maximum width after 9 h, (C) Comparison of volume after 7 h, (D) Comparison of volume after 9 h.