Pitting corrosion growth of an Inconel alloy revealed by three-dimensional reconstruction

Figure 14. Curve fitting of 3D pit feature parameters for Inconel 690 alloy immersed in 6% FeCl3 + 0.16% HCl solution at 70 °C (A) Surface area, (B) Volume, (C) Maximum width, and (D) depth vs. time for immersion duration of 10-16 h.