Non-equilibrium dendrite microstructure during quasi-rapid solidification of Mg-Al alloy

Figure 13. Change of solute concentration along the domain horizontal centerlines under different cooling rates: (A) solute trapping with solute drag; (B) solute trapping without solute drag.