fig11
Figure 11. (A) Charge density difference of the Cs3Bi2Br9/BiOBr heterojunction. Atomic force microscope (AFM) height images of (B) Cs3Bi2Br9/BiOBr. SPV images of (C) Cs3Bi2Br9/BiOBr under illumination. (A-C) Reproduced with permission from[133]. Copyright 2024, Elsevier; (D) PDOS configurations of Cs3Sb2Br9 and Cs3Mo0.13Sb1.87Br9. AFM height images of (E) Cs3Mo0.13Sb1.87Br9/BiVO4. SPV images of (F) Cs3Mo0.13Sb1.87Br9/BiVO4 under illumination. (D-F) Reproduced with permission from[134]. Copyright 2024, Elsevier; (G) Electron spin resonance spectra, (H) Nitroge temperature-programmed desorption profiles of the catalyst of Bi2MoO6 and 2% Bi2S3/Bi2MoO6. (I) Photocatalytic mechanisms of Bi2S3/OV-Bi2MoO6. (G-I) Reproduced with permission from[131]. Copyright 2022, Elsevier. PDOS: Partial density of states; SPV: surface photovoltage.