fig4
Figure 4. (A) Schematic diagram of Pb leakage test; (B) Time-dependent Pb concentration in deionized water after immersion of mechanically damaged PSCs at 25 ± 1 °C (ambient temperature); (C) Pb concentration measured for eight devices per condition; (D) Pb2+ sorption kinetics of GDY at an initial Pb2+ concentration of 10.0 ppm; the insets show the adsorbed amount and apparent first-order kinetic analysis; (E) Langmuir sorption isotherm of Pb2+ on GDY; The inset is the linearized Langmuir fit; (F) Pb 4f XPS spectra of PbI2 and PbI2+GDY; (G) FTIR spectra of GDY and GDY+PbI2; (H) Calculated adsorption energies and Pb-C bond lengths for three Pb adsorption configurations on GDY; (I) Charge-density difference map for the preferred Pb/GDY configuration. Yellow and cyan isosurfaces denote charge accumulation and charge depletion, respectively, at isovalues of ±0.001 e Å-3. PSCs: Perovskite solar cells; GDY: graphdiyne; XPS: X-ray photoelectron spectra; FTIR: Fourier-transform infrared.