fig3

High-voltage flat-tubular segment-in-series SOFCs: strategic design of an SrZrO<sub>3</sub> insulation layer

Figure 3. Phase composition, chemical compatibility, microstructure, sintering behavior, and thermomechanical properties of SZO. (A) XRD patterns of the sample sintered at 1,350 °C; (B) XRD patterns of the sample sintered at 1,350 °C and reduced at 800 °C for 12 h; (C) XRD patterns of SZO-YSZ and SZO-NiO powder mixtures after heat treatment at 1,350 °C for 4 h used to evaluate their phase compatibility; (D) SEM morphology, particle size distribution, and EDS elemental maps of SZO powder; (E) sintering behavior and apparent activation energy; (F) microstructure and elemental maps of the sintered specimen and (G) thermal expansion behavior. SZO: SrZrO3; XRD: X-ray diffraction; YSZ: yttria-stabilized zirconia; SEM: scanning electron microscopy; EDS: energy-dispersive X-ray spectroscopy.