Figure 2. High-resolution TEM images of (A) Li8VS5.5 and (B) Li8VS5.5-HC (high crystallinity) with LiVS2 and Li2S mapped in red and green, respectively. The color mapping is defined by a difference in lattice spacing. (C) Initial charge-discharge curves of ASSBs containing Li8VS5.5 and Li8VS5.5-HC under a current density of 0.13 mA cm-2 at 25 °C.