Research progress on LT performance of sodium-ion battery electrolytes

Figure 5. (A) HOMO and LUMO levels. In situ XRD of NNFMO cathodes in FPPN electrolyte: (B) Charge/discharge profiles and (C) in situ XRD patterns during cycling. (A-C) Figures reprinted with permission from Ref.[94]. Copyright 2024 Wiley-VCH. (D) Cycling performance of MN cathode in TPP and THF electrolytes at -40 °C. Reprinted with permission from Ref.[95]. Copyright 2023 The American Chemical Society. In situ sodium metal deposition in (E) BLTE and (F) ES6-BLTE electrolytes at -40 °C. Reprinted with permission from Ref.[96]. Copyright 2023 Wiley-VCH. (G) Binding energy for various Na+-solvent (PC, FEC, and TMSPi) complexes. Reprinted with permission from Ref.[97]. Copyright 2024 The American Chemical Society.

Energy Materials
ISSN 2770-5900 (Online)
Follow Us

Portico

All published articles are preserved here permanently:

https://www.portico.org/publishers/oae/

Portico

All published articles are preserved here permanently:

https://www.portico.org/publishers/oae/