fig5

Autophagy-mediated chondrocyte homeostasis: advances in hydrogel carriers for osteoarthritis treatment

Figure 5. Fabrication workflow of gefitinib-loaded hydrogels. The synthesis starts from PNIPAAm-COOH, followed by 1-ethyl-(3-dimethylaminopropyl) carbodiimide (EDC)-mediated reaction with aminated hyaluronic acid (AHA) at 4 °C for 48 h to obtain the AHA-g-PNIPAAm hydrogel. After freeze-drying, the powder is loaded with gefitinib and swollen in PBS at 4 °C for 48 h. The product is rinsed at 37 °C to yield the final gefitinib-loaded AHA-g-PNIPAAm hydrogel. EDC: 1-ethyl-(3-dimethylaminopropyl) carbodiimide; PNIPAAm: poly(N-isopropylacrylamide); AHA: aminated hyaluronic acid; PBS: phosphate-buffered saline; AHA-g-PNIPAAm: aminated hyaluronic acid-g-poly (N-isopropylacrylamide).