fig10

Figure 10. (A) Schematic of a symmetrical Li-LLZTO-Li cell depicting the orientation with respect to the external magnetic field, B0, during the 7Li CSI experiment; 7Li chemical shift images of (B) pristine and; (C) cycled Li-LLZTO-Li symmetrical cells; (D) Galvanostatic cycling at 0.5 mA cm-2 for a maximum of 2 h per discharge/charge (plating/stripping) of Li-LLZTO-Li symmetrical cells stopped for ex-situ analysis with; (E) 7Li CSI for pristine and different cycling time. Copyright 2019, American Chemical Society[101]. CSI: Chemical shift imaging.