fig2
Figure 2. (A) Stress impedance performance and (B) soft magnetic properties of the as-prepared sample and those annealed at 573, 823, and 858 K, respectively. (C) Stress impedance performance of samples with different holding times at 823 K. (D) Magnetostriction of the as-prepared ribbon and those annealed at 573, 823, 858 and 893 K, respectively.