High energy storage properties of 0.94Bi<sub>0.5</sub>Na<sub>0.5</sub>TiO<sub>3</sub>-0.06BaTiO<sub>3</sub> ceramics by incorporating <InlineParagraph>Sr<sub>0.8</sub>Bi<sub>0.1γ0.1</sub>Ti<sub>0.8</sub>Zr<sub>0.2</sub>O<sub>2.95</sub></InlineParagraph>

Figure 6. Temperature stability and fatigue resistance of the sintered ceramics. (A) P-E hysteresis loops at 25 °C to 140 °C; (B) Wr and η as a function of temperature; (C) fatigue behavior measured at various electrical cycles; (D) Wr and η as a function of electrical cycles.