Figure 7. (A) Temperature-dependent P-E loops and corresponding (C) Wrec, η of PBZ films at 1 kHz. (B) Frequency-dependent P-E loops and corresponding (D) Wrec, η of PBZ films at room temperature. PBZ: (Pb0.95Bi0.05)ZrO3.