fig4

High strength and ductility in partially recrystallized Fe<sub>40</sub>Mn<sub>20</sub>Cr<sub>20</sub>Ni<sub>20</sub> high-entropy alloys at cryogenic temperature

Figure 4. Microstructures of Fe40Mn20Cr20Ni20 HEA at different temperatures with annealing for 2 h: (A) 600 °C; (B) 700 °C; (C) 800 °C; (D) 900 °C. HEA: High-entropy alloy.