fig13

Figure 13. Optimization of solution and aging temperatures of A356-0.54Sc (Al-7.0Si-0.4Mg-0.54Sc, in wt%) alloy driven by CT approach, and the corresponding experimental verification. (A) Calculated property diagram of A356-0.54Sc alloy; (B) measured mechanical properties of A356-0.54Sc alloys with different treatments; (C-F) backscattered electron images of A356 alloys with different heat treatments. Figure reproduced from Ref.[102] with permission from Elsevier.