Figure 5. SEM images of fracture surfaces of (A) pristine NZSP; (B) 1LN; (C) 2LN; (D) 5LN; and (E) 10LN samples. The LN-modified NZSP samples exhibit predominantly transgranular fracture. SEM: Scanning electron microscope; NZSP: Na3.4Zr2Si2.4P0.6O12; LN: LaNbO4.