fig4
Figure 4. Mechanical characterization of pristine and LN-modified NZSP samples. (A and B) Elastic modulus and hardness as a function of indentation contact depth; (C) Fracture toughness values of all samples; (D and E) Representative SEM images of micropillars before and after splitting for pristine NZSP and 2LN, respectively. Error bars represent the standard deviation (SD) of measurements on one representative pellet per composition (n ≥ 36 indentations for A and B; n ≥ 6 micropillars for C). The 2LN and 5LN samples exhibit the highest elastic modulus, hardness and fracture toughness. LN: LaNbO4; NZSP: Na3.4Zr2Si2.4P0.6O12.