fig6
Figure 6. Cross-sectional SEM images and corresponding EDX images of (A) bare Li and (B) coated Li after 5 cycles of plating/stripping at 0.1 mA cm-2 with a cycling capacity of 1 mAh cm-2.
Figure 6. Cross-sectional SEM images and corresponding EDX images of (A) bare Li and (B) coated Li after 5 cycles of plating/stripping at 0.1 mA cm-2 with a cycling capacity of 1 mAh cm-2.