Design of a polymer electrolyte membrane for enhanced zinc anode stability in reversible aqueous zinc-ion batteries

Figure 5. SEM images of Zn anode in Zn|| Zn cells after long cycles in different electrolytes: (A) 1% TAC and (B) 0% TAC in Zn(CF3SO3)2, (C) 1% TAC and (D) 0% TAC in Zn(OAc)2, and (E) 1% TAC and (F) 0% TAC in ZnCl2; Galvanostatic Zn stripping and plating in a Zn||Zn cell using TAC with 1 mAh cm-2 capacity limitation in the electrolyte of (G) Zn(CF3SO3)2 under current density of 0.5 mA cm-2, and (H) Zn(OAc)2 under current density of 2 mA cm-2.