fig9
Figure 9. (A) Photograph of the OM catalyst integrated into a commercial cordierite honeycomb monolith. Reproduced with permission from Ref.[94]; (B) Changes in Pt loading of PtSA/CeZrO2 catalysts after aging at 800 and 1,100 °C. Reproduced with permission from Ref.[94]; (C) Schematic diagram illustrating the inhibitory effect of the OM structure on Pt loss during propane oxidation. Reproduced with permission from Ref.[94]. OM: Ordered macroporous; DOC: diesel oxidation catalyst.