fig5

Top-down synthesis of three-dimensional ABO<sub>3</sub>-type perovskite oxides with rich grain boundaries and lattice defects for molecular oxygen activation in catalytic oxidation reactions

Figure 5. (A) EA conversion, (B) CO2 yield and (C) the Arrhenius plots of EA oxidation over the samples; Effects of 5.0 vol% vapor on EA oxidation over (D) LMO-S, (E) La3Mn2O7, and (F) LMO-E conducted under the conditions: 200 °C, 70,000 h-1 WHSV and 1,000 ppm EA; (G) the water contact angle tests of LMO-E, LMO-S and La3Mn2O7; (H) long-term stability and (I) recyclability of the LMO-E for EA oxidation. EA: Ethyl acetate; LMO-S: LaMnO3 prepared by the sol-gel method; LMO-E: LaMnO3 prepared by the “top down” method; WHSV: weight hourly space velocities.